Fractography Study on Carbon Diffusion in Molybdenum

Jun Takada

Research output: Contribution to journalArticle

Original languageEnglish
Pages (from-to)76-83
Number of pages8
JournalProceedings of International Workshop on Designing of Interfacial Structures in Advanced Materials and their Joints
Publication statusPublished - 2003