Abstract
Objective: The purpose of this study was to investigate if incremental-filling technique and cavity size would affect the bond strength of resin composite. Methods: Two sizes of Class I cavities were prepared in bovine dentin (large cavities: π × (5/2)2 × 5 mm3; small cavity: π × (3/2)2 × 3 mm3). Light-cure resin composite (Clearfil Photocore) with a self-etching primer adhesive (Clearfil SE Bond) was placed into the cavities by bulk filling (C-factor = 5) or incremental filling (two layers, C-factor = 3) and light-cured. As a control, 3 or 5 mm thick resin composite was bonded to the flat dentin surface. After 24 h storage in 37 °C water, the micro-tensile bond strength was measured at a crosshead speed of 1 mm/min. The results obtained were statistically analyzed using two-way ANOVA and t-test at a significance level of P = 0.05. Results: The results obtained showed that there was no significant difference among the filling techniques in small cavities (P > 0.05). However, in large cavities, bulk filling presented the lowest bond strength (P < 0.05). Significance: Not only the filling technique affected the bonding strength to the cavity floor, but the cavity size was also an influential factor in Class I cavities.
| Original language | English |
|---|---|
| Pages (from-to) | 533-538 |
| Number of pages | 6 |
| Journal | Dental Materials |
| Volume | 23 |
| Issue number | 5 |
| DOIs | |
| Publication status | Published - Apr 2007 |
| Externally published | Yes |
Keywords
- C-factor
- Cavity size
- Incremental technique
- Micro-tensile bond strength
- Self-etching primer
ASJC Scopus subject areas
- General Materials Science
- General Dentistry
- Mechanics of Materials
Fingerprint
Dive into the research topics of 'The effects of cavity size and incremental technique on micro-tensile bond strength of resin composite in Class I cavities'. Together they form a unique fingerprint.Cite this
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS