N2 - Photon emission (PE) at wavelength ranges of 430-490 nm (B-PE), 500-600 nm (G-PE) and 610-680 nm (R-PE) caused by brittle fracture was simultaneously measured in the nanosecond-to-microsecond and millisecond time domains for two types of borosilicate glasses: Pyrex-type Tempax glass and BK7 glass. The results were compared to those for silica and soda lime glasses. The time dependence of the PE of Tempax glass was similar to that of silica glass, while the PE intensity was lower. Because Tempax glass contains both silica-rich and borate-rich amorphous phases, the PE must be mainly produced by the fracture of the silica-rich phase. Moreover, the proportion of B-PE of Tempax glass was higher than that of silica glass. This suggests that the measured B-PE might also include very weak PE caused by the fracture of the borate-rich phase. The PE time dependence of BK7 glass was similar to that of soda lime glass, which was different from the case for Tempax glass. The PE intensity of BK7 glass was slightly higher than that of soda lime glass, but much lower than that of Tempax glass. The result indicates that non-bridging oxygen in the glasses affects crack propagation behavior and reduces the PE.
AB - Photon emission (PE) at wavelength ranges of 430-490 nm (B-PE), 500-600 nm (G-PE) and 610-680 nm (R-PE) caused by brittle fracture was simultaneously measured in the nanosecond-to-microsecond and millisecond time domains for two types of borosilicate glasses: Pyrex-type Tempax glass and BK7 glass. The results were compared to those for silica and soda lime glasses. The time dependence of the PE of Tempax glass was similar to that of silica glass, while the PE intensity was lower. Because Tempax glass contains both silica-rich and borate-rich amorphous phases, the PE must be mainly produced by the fracture of the silica-rich phase. Moreover, the proportion of B-PE of Tempax glass was higher than that of silica glass. This suggests that the measured B-PE might also include very weak PE caused by the fracture of the borate-rich phase. The PE time dependence of BK7 glass was similar to that of soda lime glass, which was different from the case for Tempax glass. The PE intensity of BK7 glass was slightly higher than that of soda lime glass, but much lower than that of Tempax glass. The result indicates that non-bridging oxygen in the glasses affects crack propagation behavior and reduces the PE.
KW - Borosilicate glass
KW - Brittle fracture
KW - Photon emission
KW - Time-resolved measurement
UR - http://www.scopus.com/inward/record.url?scp=84957000578&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=84957000578&partnerID=8YFLogxK
U2 - 10.1016/j.jlumin.2016.01.019
DO - 10.1016/j.jlumin.2016.01.019
M3 - Article
AN - SCOPUS:84957000578
SN - 0022-2313
VL - 173
SP - 208
EP - 212
JO - Journal of Luminescence
JF - Journal of Luminescence
ER -